  2. Sampling and laboratory

Sampling and laboratory

Each lot is sampled twice and the final sample is split into three equal parts: one for you, one for the plant and one for umpire assay.

The grade is measured on a sample that represents the whole lot, not on a handful of ore.

That is why each lot is sampled at two points: first the ore crushed to 3/8 inch is quartered, and then the sample ground to 100 mesh is split. The final sample gives three equal parts: one for you, one for the plant's records and one for umpire assay.

Our laboratory delivers its results in 10 hours, depending on the day's workload.

1Quartering of the crushed ore

It is the classic method for reducing a large lot to a small sample without losing representativeness.

  1. Homogenisation

    The ore is piled into a cone and mixed with a shovel so that it is uniform.

  2. Flattening

    The cone is flattened into a round cake of even height.

  3. Division into four

    The cake is divided into four equal parts with two cross-shaped cuts.

  4. Selection

    Two opposite quarters, half of the ore, form the sample that goes to the laboratory. The other two are discarded. If necessary, this is repeated until the required sample weight is reached.

2Grinding to 100 mesh

150 µm 100 mesh 70 µm hair

To scale: the large circle is the coarsest particle that passes 100 mesh; the golden one is the thickness of a human hair.

After grinding, the ore passes through 100 mesh: particles of 150 microns or less, barely twice as thick as a human hair.

With the ore this fine, every gram of the sample closely resembles any other gram of the lot. This is the moment to take the fine samples that go to the laboratory.

3One sample, three equal parts

After the mill, a sample splitter divides the fine sample into three parts with the same weight and the same composition.

  1. For the owner of the ore

    Seller

    You take it with you, to have it analysed at the laboratory of your choice and compare results.

  2. For the plant's records

    Internal control

    Our laboratory analyses it. Results are ready in 10 hours, depending on the day's workload.

  3. For umpire assay

    Third parties and legal backing

    It is kept as a counter-sample. If the seller's and the plant's results do not match, an independent laboratory analyses it and its result is final.

Stored counter-samples. The samples of each lot are kept at the plant, so there is always material to repeat an analysis.

4Controlled grade blending

We receive high- and low-grade ore. Before going into leaching, the lots are blended to a head grade of around 20 g/t gold, always below 31 g/t, which is the limit of the circuit. The laboratory confirms the head grade before the tanks are fed.

Try a blend

Change the grades and tonnages to see the resulting head grade. It starts with the grades from the plant's example: 68 g/t and 5 g/t.

High-grade ore

Low-grade ore

Head grade of the blend 20.0g/t Au 21 t of blend
At the target gradeWith the head grade confirmed by the laboratory, the blend goes to leaching.

This is an illustrative example. At the plant, the laboratory sets the blend using the results of each lot.

5Control during leaching

In the tanks, the pulp is sampled every 30 minutes and every 2 hours. At each check, gold and silver are analysed in the solution and in the loaded carbon, and the recovery is calculated.

Classification
< 74 µm200 mesh, hydrocyclone overflow
Pulp pH
10.5 to 11.0Adjusted with lime (CaO)
Sodium cyanide
300 to 500 ppmMeasured and dosed every 2 h
Pulp sampling
30 min and 2 hSolids, solution and carbon
Laboratory building next to the leaching tanks
Plant laboratory
Staff with protective equipment next to the ball mill
Plant team in the grinding area